Copyright © 2008-2009 Badger Metal Tech, Inc – Rev 03-2009
Return to Home
First Slide
Flow Effect v/s Cavitation
Flat Surface
1.Fast flow
2.Uneven solidification
3.Erosion prone
4.Cavitation effect
When metal rushes over a flat surface, the trapped void atmosphere in low pressure areas collapse on the die surface resulting in erosion and breakout.