Historical Evidence
ØCastings tell us the bubble story
breakout prevalent at low pressure areas
gate, rebound, and flow direction changes
ØEveryday we see damage caused by cavitation
damage that was attributed to bad steel, heat treat, erosion
ØLook at tooling to see if your breakout issues correlate